Ishlab chiqarish usuli bo'yicha tasniflash
● Uzluksiz
● Payvandlangan
Payvandlash usuli bo'yicha tasniflash
● ERW
● SAWL
● SSAW
Hajm doirasi
| Turi | OD | Qalinligi |
| UZLUKSIZ | Ø33.4-323.9 mm (1-12 dyuym) | 4,5-55 mm |
| ERW | Ø21.3-609.6 mm (1/2-24 dyuym) | 8-50 mm |
| SAWL | Ø457.2-1422.4 mm (16-56 dyuym) | 8-50 mm |
| SSAW | Ø219.1-3500 mm (8-137.8 dyuym) | 6-25.4 mm |
Ekvivalent baholar
| Standart | Baho | |||||||||
| API 5L | A25 | Gr A | GrB | X42 | X46 | X52 | X56 | 60 | 65 | 70 |
| GB/T 9711 ISO 3183 | L175 | L210 | L245 | L290 | L320 | L360 | L390 | L415 | L450 | L485 |
Kimyoviy tarkibi
t ≤ 0.984" bo'lgan PSL 1 quvurining kimyoviy tarkibi
| Chelik darajasi | Massa ulushi, % issiqlik va mahsulot tahlillari asosida a, g | |||||||
| C | Mn | P | S | V | Nb | Ti | ||
| maksimal b | maksimal b | maksimal | maksimal | maksimal | maksimal | maksimal | ||
| Choksiz quvur | ||||||||
| A | 0.22 | 0.9 | 0.3 | 0.3 | – | – | – | |
| B | 0,28 | 1.2 | 0.3 | 0.3 | c,d | c,d | d | |
| X42 | 0,28 | 1.3 | 0.3 | 0.3 | d | d | d | |
| X46 | 0,28 | 1.4 | 0.3 | 0.3 | d | d | d | |
| X52 | 0,28 | 1.4 | 0.3 | 0.3 | d | d | d | |
| X56 | 0,28 | 1.4 | 0.3 | 0.3 | d | d | d | |
| X60 | 0.28 e | 1.40 e | 0.3 | 0.3 | f | f | f | |
| X65 | 0.28 e | 1.40 e | 0.3 | 0.3 | f | f | f | |
| X70 | 0.28 e | 1.40 e | 0.3 | 0.3 | f | f | f | |
| Payvandlangan quvur | ||||||||
| A | 0.22 | 0.9 | 0.3 | 0.3 | – | – | – | |
| B | 0,26 | 1.2 | 0.3 | 0.3 | c,d | c,d | d | |
| X42 | 0,26 | 1.3 | 0.3 | 0.3 | d | d | d | |
| X46 | 0,26 | 1.4 | 0.3 | 0.3 | d | d | d | |
| X52 | 0,26 | 1.4 | 0.3 | 0.3 | d | d | d | |
| X56 | 0,26 | 1.4 | 0.3 | 0.3 | d | d | d | |
| X60 | 0.26 e | 1.40 e | 0.3 | 0.3 | f | f | f | |
| X65 | 0.26 e | 1.45 e | 0.3 | 0.3 | f | f | f | |
| X70 | 0.26e | 1.65 e | 0.3 | 0.3 | f | f | f | |
a. Cu ≤ = 0,50% Ni; ≤ 0,50%; Cr ≤ 0,50%; va Mo ≤ 0,15%,
b. Uglerodning belgilangan maksimal konsentratsiyasidan 0,01% ga past har bir pasayish uchun Mn uchun belgilangan maksimal konsentratsiyadan 0,05% ga yuqoriroqqa, ≥ L245 yoki B darajalari uchun maksimal 1,65% gacha, lekin ≤ L360 yoki X52 darajalari uchun maksimal 1,75% gacha, lekin > L360 yoki X52 darajalari uchun maksimal 1,75% gacha, lekin < L485 yoki X70 darajalari uchun maksimal 2,00% gacha oshirishga ruxsat beriladi.
c. Agar boshqacha kelishilmagan bo'lsa, NB + V ≤ 0.06%
d. Nb + V + TI ≤ 0.15%,
e. Agar boshqacha kelishilmagan bo'lsa,
f. Agar boshqacha kelishilmagan bo'lsa, NB + V = Ti ≤ 0.15%,
g. B ni ataylab qo'shishga ruxsat berilmaydi va qoldiq B ≤ 0,001%
t ≤ 0.984 bo'lgan PSL 2 quvurining kimyoviy tarkibi
| Chelik darajasi | Massa ulushi, issiqlik va mahsulot tahlillari asosida % | Uglerod ekvivalenti | |||||||||
| C | Si | Mn | P | S | V | Nb | Ti | Boshqa | Idoralar IIW | Idoralar Pcm | |
| maksimal b | maksimal | maksimal b | maksimal | maksimal | maksimal | maksimal | maksimal | maksimal | maksimal | ||
| Choksiz quvur | |||||||||||
| BR | 0,24 | 0.4 | 1.2 | 0,025 | 0,015 | c | c | 0.04 | e,l | 0.43 | 0,25 |
| X42R | 0,24 | 0.4 | 1.2 | 0,025 | 0,015 | 0.06 | 0,05 | 0.04 | e,l | 0.43 | 0,25 |
| BN | 0,24 | 0.4 | 1.2 | 0,025 | 0,015 | c | c | 0.04 | e,l | 0.43 | 0,25 |
| X42N | 0,24 | 0.4 | 1.2 | 0,025 | 0,015 | 0.06 | 0,05 | 0.04 | e,l | 0.43 | 0,25 |
| X46N | 0,24 | 0.4 | 1.4 | 0,025 | 0,015 | 0.07 | 0,05 | 0.04 | d,e,l | 0.43 | 0,25 |
| X52N | 0,24 | 0.45 | 1.4 | 0,025 | 0,015 | 0.1 | 0,05 | 0.04 | d,e,l | 0.43 | 0,25 |
| X56N | 0,24 | 0.45 | 1.4 | 0,025 | 0,015 | 0.10f | 0,05 | 0.04 | d,e,l | 0.43 | 0,25 |
| X60N | 0.24f | 0.45f | 1.40 fut | 0,025 | 0,015 | 0.10f | 0.05f | 0.04f | g,h,l | Kelishilganidek | |
| BQ | 0.18 | 0.45 | 1.4 | 0,025 | 0,015 | 0,05 | 0,05 | 0.04 | e,l | 0.43 | 0,25 |
| X42Q | 0.18 | 0.45 | 1.4 | 0,025 | 0,015 | 0,05 | 0,05 | 0.04 | e,l | 0.43 | 0,25 |
| X46Q | 0.18 | 0.45 | 1.4 | 0,025 | 0,015 | 0,05 | 0,05 | 0.04 | e,l | 0.43 | 0,25 |
| X52Q | 0.18 | 0.45 | 1.5 | 0,025 | 0,015 | 0,05 | 0,05 | 0.04 | e,l | 0.43 | 0,25 |
| X56Q | 0.18 | 0.45f | 1.5 | 0,025 | 0,015 | 0.07 | 0,05 | 0.04 | e,l | 0.43 | 0,25 |
| X60Q | 0.18f | 0.45f | 1.70 fut | 0,025 | 0,015 | g | g | g | h,l | 0.43 | 0,25 |
| X65Q | 0.18f | 0.45f | 1.70 fut | 0,025 | 0,015 | g | g | g | h,l | 0.43 | 0,25 |
| X70Q | 0.18f | 0.45f | 1.80 fut | 0,025 | 0,015 | g | g | g | h,l | 0.43 | 0,25 |
| X80Q | 0.18f | 0.45f | 1.90 fut | 0,025 | 0,015 | g | g | g | i,j | Kelishilganidek | |
| X90Q | 0.16f | 0.45f | 1.9 | 0.02 | 0.01 | g | g | g | j,k | Kelishilganidek | |
| X100Q | 0.16f | 0.45f | 1.9 | 0.02 | 0.01 | g | g | g | j,k | Kelishilganidek | |
| Payvandlangan quvur | |||||||||||
| BM | 0.22 | 0.45 | 1.2 | 0,025 | 0,015 | 0,05 | 0,05 | 0.04 | e,l | 0.43 | 0,25 |
| X42M | 0.22 | 0.45 | 1.3 | 0,025 | 0,015 | 0,05 | 0,05 | 0.04 | e,l | 0.43 | 0,25 |
| X46M | 0.22 | 0.45 | 1.3 | 0,025 | 0,015 | 0,05 | 0,05 | 0.04 | e,l | 0.43 | 0,25 |
| X52M | 0.22 | 0.45 | 1.4 | 0,025 | 0,015 | d | d | d | e,l | 0.43 | 0,25 |
| X56M | 0.22 | 0.45f | 1.4 | 0,025 | 0,015 | d | d | d | e,l | 0.43 | 0,25 |
| X60M | 0.12f | 0.45f | 1.60 fut | 0,025 | 0,015 | g | g | g | h,l | 0.43 | 0,25 |
| X65M | 0.12f | 0.45f | 1.60 fut | 0,025 | 0,015 | g | g | g | h,l | 0.43 | 0,25 |
| X70M | 0.12f | 0.45f | 1.70 fut | 0,025 | 0,015 | g | g | g | h,l | 0.43 | 0,25 |
| X80M | 0.12f | 0.45f | 1.85f | 0,025 | 0,015 | g | g | g | i,j | .043f | 0,25 |
| X90M | 0.1 | 0,55 fut | 2.10f | 0.02 | 0.01 | g | g | g | i,j | – | 0,25 |
| X100M | 0.1 | 0,55 fut | 2.10f | 0.02 | 0.01 | g | g | g | i,j | – | 0,25 |
a. SMLS t>0.787", CE chegaralari kelishilgan holda belgilanadi. CEIIW chegaralari C > 0.12% ga nisbatan qo'llaniladi va CEPcm chegaralari C ≤ 0.12% bo'lsa qo'llaniladi.
b. C uchun belgilangan maksimal qiymatdan 0,01% gacha har bir pasayish uchun Mn uchun belgilangan maksimal qiymatdan 0,05% gacha oshishiga ruxsat beriladi, ≥ L245 yoki B darajalari uchun maksimal 1,65% gacha, lekin ≤ L360 yoki X52 darajalari uchun; > L360 yoki X52 darajalari uchun maksimal 1,75% gacha, lekin < L485 yoki X70 darajalari uchun; ≥ L485 yoki X70 darajalari uchun maksimal 2,00% gacha, lekin ≤ L555 yoki X80 darajalari uchun; va > L555 yoki X80 darajalari uchun maksimal 2,20% gacha.,
c. Agar boshqacha kelishilmagan bo'lsa, Nb = V ≤ 0.06%
d. Nb = V = Ti ≤ 0.15%,
e. Agar boshqacha kelishuv bo'lmasa, Cu ≤ 0,50%; Ni ≤ 0,30% Cr ≤ 0,30% va Mo ≤ 0,15%,
f. Agar boshqacha kelishilmagan bo'lsa,
g. Agar boshqacha kelishilmagan bo'lsa, Nb + V + Ti ≤ 0,15%,
h. Agar boshqacha kelishib olinmasa, Cu ≤ 0,50% Ni ≤ 0,50% Cr ≤ 0,50% va MO ≤ 0,50%,
i. Agar boshqacha kelishib olinmasa, Cu ≤ 0,50% Ni ≤ 1,00% Cr ≤ 0,50% va MO ≤ 0,50%,
j. B ≤ 0,004%,
k. Agar boshqacha kelishib olinmasa, Cu ≤ 0,50% Ni ≤ 1,00% Cr ≤ 0,55% va MO ≤ 0,80%,
l. Izohlar j bilan belgilangan navlardan tashqari barcha PSL 2 quvur navlari uchun quyidagilar qo'llaniladi. Agar boshqacha kelishilmagan bo'lsa, B ni ataylab qo'shishga ruxsat berilmaydi va qoldiq B ≤ 0,001%.
API 5l ning mexanik xususiyati
PSL 1 quvuri uchun cho'zilish sinovlari natijalariga qo'yiladigan talablar
| Quvur darajasi | Chidamlilik kuchi a | Cho'zilish kuchi a | Uzayish | Cho'zilish kuchi b |
| Rt0,5 PSI Min | Rm PSI Min | (2 dyuym Af % min da) | Rm PSI Min | |
| A | 30 500 | 48 600 | c | 48 600 |
| B | 35 500 | 60 200 | c | 60 200 |
| X42 | 42 100 | 60 200 | c | 60 200 |
| X46 | 46 400 | 63,100 | c | 63,100 |
| X52 | 52,200 | 66,700 | c | 66,700 |
| X56 | 56,600 | 71,100 | c | 71,100 |
| X60 | 60 200 | 75,400 | c | 75,400 |
| X65 | 65,300 | 77 500 | c | 77 500 |
| X70 | 70 300 | 82 700 | c | 82 700 |
| a. O'rta darajadagi novda uchun, belgilangan minimal cho'zilish kuchi va quvur korpusi uchun belgilangan minimal oqim o'rtasidagi farq keyingi yuqori darajadagi novda uchun berilganidek bo'lishi kerak. | ||||
| b. O'rta darajadagi graduslar uchun payvand chokining belgilangan minimal cho'zilish kuchi a oyoq belgisi yordamida korpus uchun aniqlangan kuch bilan bir xil bo'lishi kerak. | ||||
| c. Belgilangan minimal bo'shliqqa, Af, foizda ifodalangan va eng yaqin foizgacha yaxlitlangan holda, quyidagi tenglama yordamida aniqlanadi: | ||||
| Bu yerda C Si birliklari yordamida hisoblash uchun 1 940 ga va USC birliklari yordamida hisoblash uchun 625 000 ga teng. | ||||
| Axc - bu qo'llaniladigan cho'zilish sinov qismining ko'ndalang kesimining maydoni bo'lib, kvadrat millimetrda (kvadrat dyuym) quyidagicha ifodalanadi. | ||||
| – Dumaloq ko'ndalang kesimli sinov qismlari uchun, 12,7 mm (0,500 dyuym) va 8,9 mm (0,350 dyuym) diametrli sinov qismlari uchun 130 mm2 (0,20 dyuym2); va 6,4 mm (0,250 dyuym) diametrli sinov qismlari uchun 65 mm2 (0,10 dyuym2). | ||||
| – To'liq kesimli sinov qismlari uchun, a) 485 mm2 (0.75 dyuym2) va b) sinov qismining ko'ndalang kesim maydonining kichikroq qiymati, belgilangan tashqi diametr va quvurning belgilangan devor qalinligidan foydalanib olingan, eng yaqin 10 mm2 (0.10 dyuym2) gacha yaxlitlanadi. | ||||
| – Sinov bo'laklari uchun, a) 485 mm2 (0.75 dyuym2) va b) sinov bo'lagining ko'ndalang kesim maydonining kichikroq qiymati, sinov bo'lagining belgilangan kengligi va quvurning belgilangan devor qalinligidan foydalanib olingan, eng yaqin 10 mm2 (0.10 dyuym2) gacha yaxlitlangan. | ||||
| U - belgilangan minimal cho'zilish kuchi, megapaskallarda ifodalangan (kvadrat dyuym uchun funt) | ||||
PSL 2 quvuri uchun cho'zilish sinovlari natijalariga qo'yiladigan talablar
| Quvur darajasi | Chidamlilik kuchi a | Cho'zilish kuchi a | a,c nisbati | Uzayish | Cho'zilish kuchi d | ||
| Rt0,5 PSI Min | Rm PSI Min | R10,5IRm | (2 dyuymda) | Rm (psi) | |||
| Minimal | Maksimal | Minimal | Maksimal | Maksimal | Minimal | Minimal | |
| BR, BN,BQ,BM | 35 500 | 65,300 | 60 200 | 95 000 | 0.93 | f | 60 200 |
| X42,X42R,X2Q,X42M | 42 100 | 71 800 | 60 200 | 95 000 | 0.93 | f | 60 200 |
| X46N,X46Q,X46M | 46 400 | 76,100 | 63,100 | 95 000 | 0.93 | f | 63,100 |
| X52N,X52Q,X52M | 52,200 | 76 900 | 66,700 | 110 200 | 0.93 | f | 66,700 |
| X56N,X56Q,X56M | 56,600 | 79 000 | 71,100 | 110 200 | 0.93 | f | 71,100 |
| X60N,X60Q,S60M | 60 200 | 81 900 | 75,400 | 110 200 | 0.93 | f | 75,400 |
| X65Q,X65M | 65,300 | 87 000 | 77 600 | 110 200 | 0.93 | f | 76,600 |
| X70Q, X65M | 70 300 | 92,100 | 82 700 | 110 200 | 0.93 | f | 82 700 |
| X80Q,X80M | 80,.500 | 102,300 | 90 600 | 119,700 | 0.93 | f | 90 600 |
| a. O'rta daraja uchun to'liq API5L spetsifikatsiyasiga qarang. | |||||||
| b. > X90 darajalari uchun to'liq API5L spetsifikatsiyasiga qarang. | |||||||
| c. Bu cheklov D> 12.750 dyuymli piroglar uchun amal qiladi | |||||||
| d. O'rta darajadagi graduslar uchun payvand choki uchun belgilangan minimal cho'zilish kuchi quvur korpusi uchun a oyog'i yordamida aniqlangan qiymat bilan bir xil bo'lishi kerak. | |||||||
| e. uzunlamasına sinovni talab qiladigan quvur uchun maksimal oqim kuchi ≤ 71,800 psi bo'lishi kerak | |||||||
| f. Belgilangan minimal bo'shliqqa, Af, foizda ifodalangan va eng yaqin foizgacha yaxlitlangan holda, quyidagi tenglama yordamida aniqlanadi: | |||||||
| Bu yerda C Si birliklari yordamida hisoblash uchun 1 940 ga va USC birliklari yordamida hisoblash uchun 625 000 ga teng. | |||||||
| Axc - bu qo'llaniladigan cho'zilish sinov qismining ko'ndalang kesim maydoni bo'lib, kvadrat millimetrda (kvadrat dyuym) quyidagicha ifodalanadi. | |||||||
| – Dumaloq ko'ndalang kesimli sinov qismlari uchun, 12,7 mm (0,500 dyuym) va 8,9 mm (0,350 dyuym) diametrli sinov qismlari uchun 130 mm2 (0,20 dyuym2); va 6,4 mm (0,250 dyuym) diametrli sinov qismlari uchun 65 mm2 (0,10 dyuym2). | |||||||
| – To'liq kesimli sinov qismlari uchun, a) 485 mm2 (0.75 dyuym2) va b) sinov qismining ko'ndalang kesim maydonining kichikroq qiymati, belgilangan tashqi diametr va quvurning belgilangan devor qalinligidan foydalanib olingan, eng yaqin 10 mm2 (0.10 dyuym2) gacha yaxlitlanadi. | |||||||
| – Sinov bo'laklari uchun, a) 485 mm2 (0.75 dyuym2) va b) sinov bo'lagining ko'ndalang kesim maydonining kichikroq qiymati, sinov bo'lagining belgilangan kengligi va quvurning belgilangan devor qalinligidan foydalanib olingan, eng yaqin 10 mm2 (0.10 dyuym2) gacha yaxlitlangan. | |||||||
| U - belgilangan minimal cho'zilish kuchi, megapaskallarda ifodalangan (kvadrat dyuym uchun funt) | |||||||
| g. R10,5IRm uchun quyi qiymatlar kelishuv bilan belgilanishi mumkin | |||||||
| h. > x90 baholar uchun to'liq API5L spetsifikatsiyasiga qarang. | |||||||
Ilova
Quvur liniyasi neft va tabiiy gaz sanoati uchun suv, neft va gazni tashish uchun ishlatiladi.
JINDALAI STEEL API 5L, ISO 3183 va GB/T 9711 standartlariga muvofiq malakali choksiz va payvandlangan quvur quvurlarini taqdim etadi.
Batafsil chizma
-
A106 Crosshole Sonic Logging payvandlangan naychasi
-
API 5L B darajali quvur
-
ASTM A106 B sinfidagi choksiz quvur
-
A106 GrB choksiz grouting po'lat quvurlari qoziq uchun
-
ASTM A53 Crosshole Sonic Logging (CSL) payvandlangan quvur
-
SSAW po'lat quvuri/spiral payvandlash quvuri
-
4140 qotishma po'lat quvur va AISI 4140 quvur
-
Yuqori aniqlikdagi po'lat quvur
-
ASME SA192 Qozon Quvurlari/A192 Choksiz Po'lat Quvur
-
SA210 Choksiz Po'latdan yasalgan Qozon Quvuri